Skip to content
Trimatrix Buildtech India Pvt. Ltd.

Independent laboratory evidence

Built to perform. Tested to verify.

20 results for the uPVC profile material from three independent laboratories — each with its original report.

43MPa

Tensile strength

Resistance to being pulled apart — an indicator of everyday durability of the profile material.

Shriram Institute report

0.5%

Heat reversion

Dimensional change after heating (method reference: EN 12608). Low values mean the profile stays dimensionally stable in heat.

Shriram Institute report

0.234W/mK

Thermal conductivity

How readily heat passes through the material. This is a material property, not a window U-value.

Shriram Institute report

73.37kJ/m²

Notched Charpy impact

Energy absorbed when a notched sample is struck — a measure of impact toughness.

Shriram Institute report

V-0

Vertical flammability (UL-94)

Classification of how a sample stops burning in a vertical test. V-0 does not mean the product is fireproof.

Shriram Institute report

Material test result ≠ installed system performance. These are laboratory results for samples of the uPVC profile material, valid under the stated test conditions. They are not a guarantee of installed window performance, which also depends on glass, hardware, reinforcement, fabrication and installation.

Technical test details

All results

Grouped by property. Each laboratory name links to the report the result comes from.

Mechanical

Mechanical test results
PropertyResultWhat it meansLaboratory
Tensile strength43 MPaResistance to being pulled apart — an indicator of everyday durability of the profile material.Shriram Institute
Elongation128 %How far the material stretches before breaking — indicates toughness rather than brittleness.Shriram Institute
Flexural strength49 MPaResistance to bending under load.Shriram Institute
Flexural modulus2524 MPaStiffness of the material — how much it resists flexing.Shriram Institute

Thermal

Thermal test results
PropertyResultWhat it meansLaboratory
Vicat softening temperature79 °CTemperature at which the material begins to soften under a standard load.Shriram Institute
Heat reversion0.5 %Dimensional change after heating (method reference: EN 12608). Low values mean the profile stays dimensionally stable in heat.Shriram Institute
Heat ageing150 °C / 30 minNo visible blisters, cavities, cracks or delamination reported after heat exposure.Shriram Institute
Thermal conductivity0.234 W/mKHow readily heat passes through the material. This is a material property, not a window U-value.Shriram Institute

Impact

Impact test results
PropertyResultWhat it meansLaboratory
Notched Charpy impact73.37 kJ/m²Energy absorbed when a notched sample is struck — a measure of impact toughness.Shriram Institute
Izod impact1010 J/mA second impact-toughness method.Shriram Institute
Low-temperature impactNo brittle failure at −10 °CThe material remained tough rather than brittle at low temperature.Shriram Institute

Fire

Fire test results
PropertyResultWhat it meansLaboratory
Vertical flammability (UL-94)V-0Classification of how a sample stops burning in a vertical test. V-0 does not mean the product is fireproof.Shriram Institute
Limiting oxygen index (LOI)45 %Minimum oxygen concentration needed to sustain burning. Normal air is about 21% oxygen.Shriram Institute

Colour & Chemical

Colour & Chemical test results
PropertyResultWhat it meansLaboratory
Colour fastness (weathering)Rating 6Resistance to colour change after a weathering test.Shriram Institute
Sulphuric acid resistance0.12 g weight increaseChange in weight after exposure to sulphuric acid in the test.Shriram Institute
RoHS (restricted substances)PASSTested against cadmium, lead, mercury, hexavalent chromium, PBBs, PBDEs, DEHP, BBP, DBP and DIBP.SGS India
Lead content8.5 mg/kgMeasured in the tested sample, against the RoHS limit of 1000 mg/kg.SGS India

Physical

Physical test results
PropertyResultWhat it meansLaboratory
Density1.50 g/ccMass per volume of the profile material.Shriram Institute
Density1.52 g/ccIndependent density measurement by a second laboratory.CIPET Haldia
Surface hardness81 Shore DResistance to surface indentation.CIPET Haldia

In plain language

What these tests mean for you

Thermal stability

Heat reversion of 0.5% and heat ageing at 150 °C / 30 min with no visible defects reported indicate the profile holds its shape in heat.

Everyday durability

Tensile (43 MPa) and flexural (49 MPa) strength describe how the material resists pulling and bending loads.

Low-temperature impact

No brittle failure at −10 °C — the material stays tough rather than cracking on impact.

Colour stability

Colour fastness rating 6 after the weathering test describes resistance to colour change.

Flammability testing

UL-94 V-0 and LOI 45% describe how the material behaves in standard flame tests. They do not mean the product is fireproof.

Verify the results

Tested by independent laboratories

Shriram Institute for Industrial Research

Mechanical, thermal, impact, fire and weathering tests

View test report

CIPET Haldia

Physical properties — surface hardness and density

View test report

SGS India Pvt. Ltd.

Restricted substances (RoHS)

Report No. MAN:HL:1548004308

View test report

Material test result ≠ installed system performance. These are laboratory results for samples of the uPVC profile material, valid under the stated test conditions. They are not a guarantee of installed window performance, which also depends on glass, hardware, reinforcement, fabrication and installation.

Start a conversation

Questions about the data?

Ask the Trimatrix team how these results apply to your project.

Prefer to talk? Call +91 9220420757 or email info@trimatrixbuildtech.com.